Polymer Property : Bulk Density = 0.0608 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 1.68 g/cc
0.0608 lb/in³
Packed
Excalibar ExBar™ W 2 Barite BaSO4 Powder
ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, ..
Bulk Density 1.68 g/cc
0.0608 lb/in³
Powder
Aremco Ceramacast™ 586 High Temperature Potting & Casting Material Zirconia Silicate
Castable ceramic for ceramic and metal assemblies. Excellent handling, fast curing.