Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.68 g/cc | 0.0608 lb/in³ | Packed |
Excalibar ExBar™ W 2 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Bulk Density | 1.68 g/cc | 0.0608 lb/in³ | Powder |
Aremco Ceramacast™ 586 High Temperature Potting & Casting Material Zirconia Silicate Castable ceramic for ceramic and metal assemblies. Excellent handling, fast curing. |