Polymer Property : Bulk Density = 0.106 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 2.93 g/cc
0.106 lb/in³
Poco Graphite SUPERSiC® Si Silicon Carbide
The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for..
Bulk Density 2.93 g/cc
0.106 lb/in³
Chosun Refractories A18H Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.93 g/cc
0.106 lb/in³
Chosun Refractories A18HM Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Bulk Density 2.93 g/cc
0.106 lb/in³
Chosun Refractories A18S Magnesia Carbon Bricks for Electric Arc Furnace
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).