Poco Graphite SUPERSiC® Si Silicon Carbide

Category Ceramic , Carbide
Manufacturer Poco Graphite
Trade Name SUPERSiC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite SUPERSiC® Si Silicon Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The SUPERSiC Material System allows customization of basic silicon carbide. Select from groups of infiltration materials, cleaning options, coating materials and thicknesses to optimize material for specific applications.POCO’s unique conversion process produces the highest quality silicon carbide products available on the market today. This process starts with graphite material specially designed and manufactured for use as the precursor in the conversion process. Near net parts are machined in graphite, purified, and subjected to a proprietary conversion process which substitutes pure silicon atoms for carbon atoms. The result is SUPERSIC, POCO’s high purity silicon carbide.
Physical Properties Metric English Comments
Bulk Density 2.93 g/cc
0.106 lb/in³
Apparent Bulk Density 3.01 g/cc
0.109 lb/in³
Open Porosity 0.50 %
0.50 %
Porosity 4.0 %
4.0 %
Mechanical Properties Metric English Comments
Hardness, Knoop 1643
1643
[kg/mm<sup>2</sup>]
Tensile Strength 124 MPa
18000 psi
Modulus of Elasticity 338 GPa
49000 ksi
Flexural Strength 223 MPa
32300 psi
Poissons Ratio 0.17
0.17
Fracture Toughness 2.63 MPa-m½
2.39 ksi-in½
Shear Modulus 138 GPa
20000 ksi
Dynamic
Thermal Properties Metric English Comments
CTE, linear 2.40 µm/m-°C
1.33 µin/in-°F
Thermal Conductivity 220 W/m-K
1530 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.400 ohm-cm
0.400 ohm-cm
Descriptive Properties Value Comments
Total Impurity Level (ppm), Max 10