Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.150 g/cc | 0.00542 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons DUREX® 0, Powder Carbon Black Specialty carbon black for technical rubber goods; Excellent extrusion propertiesProduced by Lamp Black processInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.150 g/cc | 0.00542 lb/in³ | |
SGL Carbon Group SIGRAFIL C® C25 M350 UNS Milled Carbon Fiber, Unsized Carbon Fiber Milled SIGRAFIL C is excellent for making materials electrically conductive such as powders, dry mixtures, adhesives, floorings, aqueous adhesive systems and all aqueous mixing processes. Milled SIG.. |
|||
Bulk Density | 0.150 g/cc | 0.00542 lb/in³ | Scott |
TIMCAL C-THERM™ 001 Graphite Additive for Thermally Conductive Polymers The C-THERM line of high aspect ratio expanded graphite is designed to be added to polymers for the purpose of increasing the thermal conductivity of the resulting compound. Graphite's phonon colli.. |
|||
Bulk Density | 0.150 g/cc | 0.00542 lb/in³ | |
American Elements Z-MITE™ Zinc Oxide Nanopowder General DescriptionZ-MITE powders are inorganic zinc-oxide nanoparticles with antibacterial, antifungal, anti-corrosion, catalytic, and UV filtering properties. Z-MITE-A products are uncoated and hy.. |
|||
Bulk Density | 0.150 g/cc | 0.00542 lb/in³ | |
Applied Nanostructured Solutions Carbon NanoStructure Chopped Fiber Carbon NanoStructure (CNS) Chopped Fiber begins as a single-end glass roving product, such as E-CR glass, that is enhanced using a proprietary ANS process. Unique multiwall carbon nanotube-based CNS.. |