Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Applied Nanostructured Solutions Carbon NanoStructure Chopped Fiber

Category Carbon , Carbon Fiber , Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Carbon Fiber Filled
Manufacturer Applied Nanostructured Solutions
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Applied Nanostructured Solutions Carbon NanoStructure Chopped Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carbon NanoStructure (CNS) Chopped Fiber begins as a single-end glass roving product, such as E-CR glass, that is enhanced using a proprietary ANS process. Unique multiwall carbon nanotube-based CNS are added to the glass surface, endowing the product with multifunctional properties. This CNS-infused chopped glass product is designed for use as a reinforcement for thermoset and thermoplastic resins that not only yields enhanced mechanical properties, but also makes the material conductive.*Properties are for PC/ABS CNS-infused glass fiber 3%Information provided by Applied Nanostructured Solutions (ANS)
Physical Properties Metric English Comments
Bulk Density 0.150 g/cc
0.00542 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength 100 MPa
14500 psi
ASTM D638
Tensile Modulus 8.96 GPa
1300 ksi
ASTM D638
Flexural Strength 140 MPa
20300 psi
ASTM D790
Flexural Modulus 8.76 GPa
1270 ksi
ASTM D790
Electrical Properties Metric English Comments
Shielding Effectiveness 35 dB

@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
35 dB

@Thickness 0.118 in,
Frequency 3.00e+7 Hz
15% glass; ASTM D4935
40 dB

@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
40 dB

@Thickness 0.118 in,
Frequency 2.03e+9 Hz
15% glass; ASTM D4935
44 dB

@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
44 dB

@Thickness 0.118 in,
Frequency 3.00e+7 Hz
25% glass; ASTM D4935
50 dB

@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
50 dB

@Thickness 0.118 in,
Frequency 2.03e+9 Hz
25% glass; ASTM D4935
51 dB

@Thickness 3.00 mm,
Frequency 3.00e+7 Hz
51 dB

@Thickness 0.118 in,
Frequency 3.00e+7 Hz
30% glass; ASTM D4935
60 dB

@Thickness 3.00 mm,
Frequency 2.03e+9 Hz
60 dB

@Thickness 0.118 in,
Frequency 2.03e+9 Hz
30% glass; ASTM D4935
Processing Properties Metric English Comments
Moisture Content <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
% Sizing, type ~5%
Polyurethane
Chop Length 6mm
Glass Tex 850
Glass Type E-CR
Users viewing this material also viewed the following: