Physical Properties Metric English Comments
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Pau Tai UNINOX AM-929 Acrylic Impact Modifier
UNINOX AM-929 is acrylic impact modified resin. It is the most efficient high impact modifier for rigid PVC and other polymers, and recommended for use in calendered sheets, extruded pipe, foam prof..
Bulk Density 0.250 - 0.450 g/cc
0.00903 - 0.0163 lb/in³
Magyar Aluminum ALOLT 90DLS Aluminum Hydroxide
Fine Precipitated Type
Bulk Density 0.200 - 0.450 g/cc
0.00723 - 0.0163 lb/in³
Magyar Aluminum ALOLT 90F Aluminum Hydroxide
Fine Precipitated Type
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ HA Hollow Spheres
EXTENDOSPHERESâ„¢ HA are off white, low-cost, low-density, high alumina, ceramic hollow spheres.Applications: Hollow spheres are ideal for use in coatings, sealants, caulks and other applications..
Bulk Density 0.300 - 0.450 g/cc
0.0108 - 0.0163 lb/in³
Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles)
Usage: The resin is mainly used as an insulating film for electric applications, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, and loop.Packing: PTFE is packed in ..
Bulk Density 0.300 - 0.450 g/cc
0.0108 - 0.0163 lb/in³
Shandong Dongyue Polymer DF-16 PTFE Molding Powder (Micronized Particles)
Usage: The resin can be used as the general required electric source, which is suitable for making film, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, loop, fillin..
Bulk Density 0.300 - 0.450 g/cc
0.0108 - 0.0163 lb/in³
Shandong Dongyue Polymer DF-17 PTFE Molding Powder (Micronized Particles)
Usage: The resin is mainly used as the packing products resource and packing pelletized resource, which can be processed to film, the products of thin wall, seal, gasket, club, panel, tube, axletree..
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Trelleborg Fillite® 160 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Trelleborg Fillite® 52/7S (355) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Trelleborg Fillite® FG (300) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Trelleborg Fillite® 106 Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..
Bulk Density 0.370 - 0.450 g/cc
0.0134 - 0.0163 lb/in³
Akzo Nobel Expancel® 930 MB 120 Masterbatch with unexpanded microspheres
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the..
Bulk Density 0.350 - 0.450 g/cc
0.0126 - 0.0163 lb/in³
Trelleborg Fillite® PG (300LF) Alumino-silicate Cenospheres
Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio..