Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.300 - 0.400 g/cc | 0.0108 - 0.0145 lb/in³ | |
Oceanchem Group Melamine Cyanurate (MCA) Molecular Formula: C6H9N9O3Cas No.: 37640-57-6Physical Appearance: Fine, white, crystalline powder, nontoxic, odorless; indissolvable in water and most organic solvents.Use: Melamine Cyanurate is a .. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
Nabaltec APYRAL® 60CD Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | ISO 1183 |
Victrex® PEEK 150XF Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, fine powder for compression moulding, easy flow, FDA food contact compliant, .. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | ISO 1183 |
Victrex® PEEK 450PF Fine Powder Grade Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia.. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Magyar Aluminum ALO-P90-02 Alumina Alumina for Polishing |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Magyar Aluminum ALO-P95-01 Alumina Alumina for Polishing |
|||
Bulk Density | 0.300 - 0.400 g/cc | 0.0108 - 0.0145 lb/in³ | ASTM D1895 |
LG Chemical PA1302 PVC General Description: PA1302, vinyl chloride copolymer with vinyl acetate exhibits excellent properties. It is easy to process and gives effective flow. Main Applications: Adhesive for sheet & film, .. |
|||
Bulk Density | 0.300 - 0.400 g/cc | 0.0108 - 0.0145 lb/in³ | ASTM D1895 |
LG Chemical PB1752 PVC General Description: PB1752, homopolymer made from micro-suspension seeded polymerization, is a low-viscosity PVC resin with a pseudo-plastic flow property in processing range. It can be used for sk.. |
|||
Bulk Density | 0.300 - 1.60 g/cc | 0.0108 - 0.0578 lb/in³ | |
GrafTech GRAFCELL® GDB Graphite Gas Diffusion Barrier GRAFCELL® Gas Diffusion Barrier (GDB) material is a thin, perforated structure made from a continuous matrix of expanded natural graphite with excellent electrical conductivity, thermal conductiv.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | Tap Density |
Momentive Performance Materials PolarTherm® PT132 Boron Nitride (BN) Powder Boron Nitride powders are produced by GE Advanced Ceramics in more than 50 individual (standard and custom) grades to meet a wide variety of application needs.For use in: Electrically insulating/the.. |
|||
Bulk Density | 0.300 - 0.600 g/cc | 0.0108 - 0.0217 lb/in³ | |
Solvay Chemicals KaCeFlux Potassium Fluoroaluminate Standard flux for brazing aluminum.HS No.: 3810100000 /CAS-No.: 60304-36-1 and 14484-69-6Uses: Automotive Sector, Commercial & Residential Air Conditioning, Refrigeration and Household & Electri.. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-521 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-732 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-760 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-870 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKEâ„¢ RK-870G MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKEâ„¢ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is .. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ 300/600 Hollow Spheres EXTENDOSPHERESâ„¢300/600 are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, they can .. |
|||
Bulk Density | 0.300 - 0.450 g/cc | 0.0108 - 0.0163 lb/in³ | |
Shandong Dongyue Polymer DF-11 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as an insulating film for electric applications, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, and loop.Packing: PTFE is packed in .. |
|||
Bulk Density | 0.300 - 0.450 g/cc | 0.0108 - 0.0163 lb/in³ | |
Shandong Dongyue Polymer DF-16 PTFE Molding Powder (Micronized Particles) Usage: The resin can be used as the general required electric source, which is suitable for making film, the products of thin wall, seal, gasket, club, panel, tube, axletree, seal ring, loop, fillin.. |
|||
Bulk Density | 0.300 - 0.450 g/cc | 0.0108 - 0.0163 lb/in³ | |
Shandong Dongyue Polymer DF-17 PTFE Molding Powder (Micronized Particles) Usage: The resin is mainly used as the packing products resource and packing pelletized resource, which can be processed to film, the products of thin wall, seal, gasket, club, panel, tube, axletree.. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Dow Corning EP-9261 TI Cosmetic Powder This cosmetic powder provides smoothness and a powdery, non-greasy skin feel; high sebum absorption; soft focus; and improves SPF. As a white cross-linked dimethyl polysiloxane elastomer powder comb.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
Azoty Tarnow™ TARFLEN SM-1 PTFE Non Free-Flowing suspension powder for standard compression molding and compounding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
BASF Paliotol™ Yellow K 1841 Color Additive Chemical Structure: Isoindoline YellowApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provide.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
Asahi Glass Fluon® L173J PTFE Lubricant Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | |
BASF Theroplast® Black X70 Color Additive Application: Colourant for plastics: PVC-u, PS, SAN, PMMA, PC, PA and UPRecommendations for food applications: BgVV, FrancePhysical form: PowderInformation provided by BASF |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | Pour Density; ASTM D 1513 |
Orion Engineered Carbons CORAX® HP 160 HP Carbon Black Specialty black designed for excellent dry grip as required for racing tiresHard Black - tread grade, reinforcing carbon blackInformation provided by Orion Engineered Carbons. |
|||
Bulk Density | 0.300 - 0.500 g/cc | 0.0108 - 0.0181 lb/in³ | |
Shandong Rike Chemical RIKE™ RK-764 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKE™ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is endo.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 7700P Fiberglass and Mineral Reinforced Phenolic Novolac FM 7700P is a two-stage phenolic molding compound reinforced with cotton fabric in pellet form. FM-7700P is recommended to customers desiring approval under ASTM D-5948-96,Type CFI-20. (Replaces Mil.. |
|||
Bulk Density | 0.300 g/cc | 0.0108 lb/in³ | ISO 1183 |
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |