Physical Properties Metric English Comments
Bulk Density 0.481 - 0.561 g/cc
0.0174 - 0.0203 lb/in³
Green Dot Terratek® WC 100300 Polypropylene - Pine Fiber Composite
Terratek® WC 100300 is a proprietary blend of pine wood fiber and reprocessed polypropylene for injection molding applications. WC 100300 contains 30% wood fiber by weight, however, a range of pr..
Bulk Density 0.481 g/cc
0.0174 lb/in³
As Supplied
Skamol Group Moler 5 Aggregate Insulation
SKAMOL insulating aggregates have the following characteristics: Max. service temperature: Up to 900°C (1652°F)Back-up insulationLightweightGood insulating propertiesChemically inertDue to fre..
Bulk Density 0.481 g/cc
0.0174 lb/in³
Dry
Skamol Group SKAMOLEX V-1100 (475) Customized Shape
SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers..
Bulk Density 0.481 g/cc
0.0174 lb/in³
Tapped
CIMBAR CIMTUFF® 9102 Talc
CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® ..