SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and versatile highly insulating refractory panels and shapes made of vermiculiteResistant to high temperatures, withstand direct flame impingementGood electrical resistivityCustomized designs: Special shapes or panels, surface pattern and two-dimensional effectsAvailable in various combinations of bulk density, insulation properties and compressive strengthHave a myriad of uses and are ideally suited for lining hearth and heating appliances such as fireplaces, gasfires and stoves as well as night storage heaters, domestic boilers, and cooking appliancesAlso used in high temperature industries where special designs are required, possibly in combination with calcium silicate slabs.Information provided by Skamol.
Physical Properties Metric English Comments
Bulk Density 0.481 g/cc
0.0174 lb/in³
Dry
Mechanical Properties Metric English Comments
Modulus of Rupture 0.000800 GPa
0.116 ksi
EN 993-6: 1995
Compressive Strength 2.50 MPa
363 psi
EN 1094-5: 1995
Thermal Properties Metric English Comments
Specific Heat Capacity 0.940 J/g-°C
0.225 BTU/lb-°F
Thermal Conductivity 0.140 W/m-K

@Temperature 200 °C
0.972 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
0.170 W/m-K

@Temperature 400 °C
1.18 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-182
0.190 W/m-K

@Temperature 600 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Maximum Service Temperature, Air 1100 °C
2010 °F
Shrinkage 1.00 %

@Temperature 1000 °C,
Time 43200 sec
1.00 %

@Temperature 1830 °F,
Time 12.0 hour
Linear Reheat Shrinkage; EN 1094-6: 1999