Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.520 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.450 - 0.520 g/cc
0.0163 - 0.0188 lb/in³
Shandong Rike Chemical HELIâ„¢ HLC-135A PVC Impact Modifier-CPE Series
Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte..
Bulk Density 0.450 - 0.520 g/cc
0.0163 - 0.0188 lb/in³
Shandong Rike Chemical HELIâ„¢ HLC-2235 PVC Impact Modifier-CPE Series
Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte..
Bulk Density 0.510 - 0.520 g/cc
0.0184 - 0.0188 lb/in³
BASF NEOL® Neolpentylglycol Flakes
Formula: C5H12O2CAS: 126-30-7Description: Neolpentylglycol (NEOL) flakes are colorless with a sweetish odor.Synonyms: Neopentanediol, 2,2-Dimethyl-1,3-propanediol, 1,3-Dihydroxy-2,2-dimethylpropane,..