Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | Tapped |
Nyco ASPECT® 3000 Wollastonite High aspect ratio grade. It is available untreated or with a surface modification treatment.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. .. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | |
Nabaltec APYMAG® 40S Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | |
Solvay Specialty Polymers Polymist® F-5 PTFE Powder Lubricant
(discontinued **) Polymist® powders are a family of white free-flowing polytetrafluoroethylene powders for use as additives in other materials to enhance processing or end-use performance characteristics. Polymist .. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | ISO 12086 |
3M Dyneon™ TFM™ 2001 PTFE
(discontinued **) Processable by standard paste extrusion methodRecommended for high performance applications with reduction ratios up to 1000:1Provides denser polymer structure with fewer micro voids and lower gas p.. |
|||
Bulk Density | 0.450 - 0.600 g/cc | 0.0163 - 0.0217 lb/in³ | |
Gromax EP-5016M Unplasticized Vinyl Acetate homopolymer Product Description: EP-5016M is a water redispersible vinyl acetate homopolymer powder that is readily dispersible in water and forms stable emulsion. This redispersible powder is especially recomm.. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | |
SGL Carbon Group CF 3100 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Bulk Density | 0.450 - 0.520 g/cc | 0.0163 - 0.0188 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HLC-135A PVC Impact Modifier-CPE Series Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte.. |
|||
Bulk Density | 0.450 - 0.520 g/cc | 0.0163 - 0.0188 lb/in³ | |
Shandong Rike Chemical HELIâ„¢ HLC-2235 PVC Impact Modifier-CPE Series Mechanism of Impact ModificationIt is found by research that the weak impact strength of PVC under lower temperature is mainly caused by stronger intermolecular force of PVC. Owing to stronger inte.. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | |
Solvay GEROPON® SC/213 Surfactant Description: Multipurpose dispersing agent for WP and WDG formulations.Identification: POTASSIUM POLYCARBOXYLATESolubility: Soluble in water. Insoluble in polar and aromatic solvents.Available in: .. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 3001 Cellulose Reinforced Phenolic Novolac FM 3001 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear. Information supplied by Sumitomo Bak North America... |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | |
Solvay RHODAPHOSE® DIPHENYL PHOSPHINO FERROCENE Phosphorus Derivative Identification: 1,1’-BIS-(DIPHENYLPHOSPHINO) FERROCENE (DPPF)CAS: 12150 – 46 – 8Available in: Asia Pacific, Europe, Latin America and North America Applications: DPPF (1,1’-Bis(d.. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | |
Solvay SOPROPHOR® S/40 FLAKES Surfactant Description: Multipurpose dispersing agent for SC formulationsIdentification: ETHOXYLATED POLYARYLPHENOLSolubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, .. |
|||
Bulk Density | 0.450 - 0.550 g/cc | 0.0163 - 0.0199 lb/in³ | Powder Density; ISO 60 |
Vyncolit 4451 XB Novolac Phenolic Organic and mineral filled phenolic molding compound with excellent mechanical properties (highest notched impact strength).USES: Fuse holders, brush holders, circuit breakers, automotive ignition a.. |
|||
Bulk Density | 0.450 - 0.550 g/cc | 0.0163 - 0.0199 lb/in³ | |
Chengdu Polyster MCA Melamine Cyanurate White crystal power with satiny. It is an excellent non-halogen N flame retardant. The product is mainly used as non-halogen flame retardant for synthetic resin(PA, PVC, PS, POM), synthetic rubber a.. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | |
DuPont™ Nomex® 419 Paper, 7 mil Nominal Thickness Nomex® Type 419 is the uncalendared precursor of Nomex® Type 418. It is used in applications in which its lower density allows improved conformability and saturability.General NOMEX Information: .. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | ASTM D-1895 |
Braskem UTEC® 3040 Ultra High Molecular Weight Polyethylene Description: UTEC3040 is an Ultra High Molecular Weight Polyethylene with a molecular weight about 10 times higher than High Density Polyethylene (HDPE) resins. This extremely high molecular weight .. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | ASTM D-1895 |
Braskem UTEC® 4040 Ultra High Molecular Weight Polyethylene Applications which require a good combination between impact and wear resistance - technical and porous parts, filters, compression molded sheets.Information provided by Braskem. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | ASTM D-1895 |
Braskem UTEC® 4041 Ultra High Molecular Weight Polyethylene Applications which require a good combination between impact and wear resistance - use of pigments and/or additives - technical and porous parts, filters, compression molded sheets.Information provi.. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | ASTM D-1895 |
Braskem UTEC® 5040 Ultra High Molecular Weight Polyethylene Applications which require high wear resistance - technical parts, RAM extruded and compression molded sheets, rods and profiles.Information provided by Braskem. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | ASTM D-1895 |
Braskem UTEC® 5041 Ultra High Molecular Weight Polyethylene Applications which require high wear resistance and the use of pigments and/or additives - technical parts, RAM extruded and compression molded sheets, rods and profiles.Information provided by Bras.. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | ASTM D-1895 |
Braskem UTEC® 6540 Ultra High Molecular Weight Polyethylene Applications which require highest wear resistance - technical parts, RAM extruded and/or compression molded sheets, rods and profiles.Information provided by Braskem. |
|||
Bulk Density | 0.450 - 0.800 g/cc | 0.0163 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Conditioned) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Bulk Density | 0.450 - 0.800 g/cc | 0.0163 - 0.0289 lb/in³ | |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | DIN EN ISO 60 |
3M Dyneon™ TFM™ 2001Z PTFE Dyneon™ TFM™ 2001 Z PTFE is an ideal grade for high-performance applications with reduction ratios up to 1000:1. This product has a denser polymer texture providing lower gas permeability than sta.. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | ASTM D1895 |
ALM D80-ST Nylon 11 SLS Prototyping Polymer Unfilled, color stabilized nylon 11 material that is also stabilized to prevent premature thermal degradation. Parts produced from PA D80-ST exhibit superior mechanical properties. Relatively inexp.. |
|||
Bulk Density | 0.450 - 0.510 g/cc | 0.0163 - 0.0184 lb/in³ | PVCH/QCD/3516 |
Reliance Industries 70-21 Polyvinyl Chloride Information provided by Reliance IndustriesApplications:Can be used:Flexible extrusionFlexible injectionFlexible calendering |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | |
Beijing Evergrow Resources UHMW PE Powder Ultra-high molecular weight polyethylene (UHMWPE) is an outstanding engineering plastic. It’s characterized by the following properties.Features:Very high abrasion resistanceVery high impact streng.. |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | Powder; ASTM D1895 |
Sumitomo Bakelite North America FM 3000 Cellulose Reinforced Phenolic Novolac FM 3000 is a self-lubricated cellulose reinforced phenolic molding compound, modified for applications requiring reduced friction and low wear. Information supplied by Sumitomo Bak North America... |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | ASTM D4745 |
3M Dyneon™ CC203 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 15% mineral blended with PTFE.Information provided by Dyneon, A 3M Company |
|||
Bulk Density | 0.450 g/cc | 0.0163 lb/in³ | |
Sharadaa Ceramics 0.4 Insulation Brick Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |