Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.529 - 0.593 g/cc | 0.0191 - 0.0214 lb/in³ | ASTM D1895 |
LyondellBasell Alathon® H5220 High Density Polyethylene, Injection Molding Grade ApplicationsAlathon H5220 provides easy processing characteristics and exhibits excellent toughness properties and color as well as low odor and good processing stability. Typical applications inclu.. |