Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | Loose |
Nyco NYAD® M400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | Loose |
Nyco NYAD® MD400 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir ICE R 830D Polystyrene Environmental stress cracking resistant (ESCR) HIPS. ICE PD R 830D combines high impact strength with an improved chemical resistance to oils, fats and chemical agents, such as detergents for both i.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir N 1782 Polystyrene General purpose polystyrene with good flow and high heat resistance. Suggested for direct gassing extrusion of heavy gage insulating boards (XPS) and in blend with high concentration of clear SBS f.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir R 321P Polystyrene Medium impact polystyrene combining easy flow and high stiffness. For injection moulding of parts with low thickness and high rigidity. Designation: Thermoplastics ISO 2897-PS-I,M,083-12-04-30Applic.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir R 540E Polystyrene HIPS with high stiffness, matt surface finish and good heat resistance. Suitable for general extrusion of thick sheets and profiles. Also used for injection
moldings. Designation: Thermoplastics IS.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir R 850E Polystyrene Super high impact polystyrene with good heat resistance. Designed for sheet extrusion and thermoforming of deep drawn containers even
diluted with high percentage of GP. Suitable for general injecti.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir SR 550 Polystyrene High impact, easy flow polystyrene with good elasticity at low temperatures.Suitable for injection moulding of large or complex parts with low thickness and high impact strength.
Designation: Thermo.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | |
Nabaltec APYRAL® 24 Al(OH)3 APYRAL ® from Nabaltec is an environmentally friendly halogen free product which is used as a flame retardant filler in a wide variety of rubber and polymeric materials. During thermal decompositio.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir RCL 600 Polystyrene
(discontinued **) Special medium impact polystyrene extrusion grade exhibiting very high gloss. This grade should be used where is required an excellent surface finish. It can be directly extruded in foils and sheets.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Styron Magnumâ„¢ 3453 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3453 ABS is a general purpose injection molding resin suitable for a wide range of applications.Information provided by DowThis product line was spun off from Dow Chemical to Styron in .. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun .. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Styron Magnumâ„¢ 3525 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3525 is a resin with excellent processing characteristics. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent processability with a stable.. |
|||
Bulk Density | 0.650 - 0.850 g/cc | 0.0235 - 0.0307 lb/in³ | RP-0155 |
Solvay REPEL-O-TEX® SF2 Surfactant Description: High active soil release polymer for powder laundry. Prevents adhesion of soils between washes and soil redeposition during wash. Repel-O-Tex SF2 has been specifically formulated for im.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Styron Magnumâ„¢ 3325 MT Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3325 MT is resin with excellent processing characteristics and a matt surface finish. The mass (continuous process) ABS technology of Dow ensures an ABS resin that combines excellent p.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Plenco 2482 Phenolic, Granular, Transfer Molded PLENCO 02482 is a general purpose, organic filled phenolic molding compound offering excellent mechanical strength while maintaining dielectric properties at elevated humidity levels. UL recognized .. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Plenco 5488 Phenolic, Granular, Injection Molded PLENCO 05488 is a woodflour and graphite filled phenolic molding compound offering improved abrasion resistance. UL recognized under component file E40654. 05488 is available in brown. 05488 is not .. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 060 |
Videolar 500 Crystal Polystyrene (GPPS) Designed for injection moldingVery easy flowing grade for fast cycle injection moldingExcellent processability for filling thin partsFeatures: Good strengthGood temperature resistanceExcellent clari.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Vyncolit Neopreg Kinel® SK61 L5G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particular suited for over molding.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | Powder Density; ISO 60 |
Vyncolit X640 Resole Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | Powder Density; ISO 60 |
Vyncolit X6952 Novolac Phenolic Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ASTM D1895 |
Plenco 6301 Phenolic, Granular, Injection Molded PLENCO 06301 is an inorganic reinforced phenolic molding compound, offering excellent heat resistance, dimensional stability, and processability as required for typical automotive applications. It i.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 060 |
Videolar 825 E High Impact Polystyrene (HIPS) Grade designed specially for extrusion and thermoformingCharacteristics make it especially suitable for industrial packaging deep draw thermoforming and custom multilayer sheet extrusionFeatures: St.. |
|||
Bulk Density | 0.650 - 0.850 g/cc | 0.0235 - 0.0307 lb/in³ | |
BASF Ultraform® N2640 Z2 POM + PUR Description: Elastomer-modified injection molding grade with high impact strength for clips, snap and fastening elements, and also for components subject to impact stress.Information provided by BAS.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | |
Daikin NEOFLON EC-6510 ETFE Coating Powder, White Description: 0.3-2.0 mm thickness.Processing Methods:Electro-static spray coating.Information provided by Daikin Industries. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir N 2982 Polystyrene General purpose polystyrene with very high flow and high heat resistance. Special grade for direct gassing extrusion of heavy gage insulating boards (XPS) foamed by blowing agents alternative to CFC.. |
|||
Bulk Density | 0.650 g/cc | 0.0235 lb/in³ | ISO 60 |
Polimeri Europa Edistir N 1910 Polystyrene Very easy flow general purpose polystyrene. Used for injection of thin-wall, multi-cavity, very fast-cycle mouldings and for sheet extrusion in glossy capping of HIPS and in blend with HIPS or clear.. |