Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.993 g/cc | 0.0359 lb/in³ | loose |
Imerys G-200 HP Feldspar G-200 HP Feldspar is a high potassium aluminum silicate ground to 200 mesh for ceramic applications. G-200 HP offers high potassium content and low iron oxide per unit of alumina.Information provide.. |
|||
Bulk Density | 0.993 g/cc | 0.0359 lb/in³ | loose |
Imerys Minsparâ„¢ 170 Feldspar Minspar170 Feldspar is a high quality sodium/ potassium/ calcium aluminum silicate ground to 170 mesh for ceramic applications. Carefully beneficiated and controlled for quality, Minspar 170 Feldspa.. |
|||
Bulk Density | 0.993 g/cc | 0.0359 lb/in³ | loose |
Imerys Minsparâ„¢ 250 Feldspar Information provided by Imerys |
|||
Bulk Density | 0.993 g/cc | 0.0359 lb/in³ | Defined by casting method, +/- 50kg (110 lbs) |
Skamol Group VERMICAST 14-100 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |