Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 1.09 g/cc | 0.0394 lb/in³ | Loose |
Excalibar ExBar™ W 3 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Bulk Density | 1.09 g/cc | 0.0394 lb/in³ | Tapped |
CIMBAR CIMTUFF® 9110 Talc CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® .. |
|||
Bulk Density | 1.09 g/cc | 0.0394 lb/in³ | Tapped |
CIMBAR MV 610 Talc MV Series talcs are produced from high purity talc ore, which provide good color, acid resistance and excellent barrier properties when used in paint & coating formulations. MV Series talcs are pla.. |
|||
Bulk Density | 1.09 g/cc | 0.0394 lb/in³ | Tapped |
CIMBAR RP 9405 Talc RP 9400 Series talcs are produced from ores, which provide an excellent balance of mechanical properties at an economical price, for primary use in commodity polypropylene. RP 9400 Series talcs are.. |