CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® 9100 Series talcs are primarily used in performance polypropylene, where improved tensile strength, flexural modulus, heat distortion temperature, increased stiffness, reduced shrinkage and lower compounding costs are required. CIMTUFF® 9100 Series talcs are platy, hydrophobic, non-abrasive and chemically inert.Information provided by Cimbar Performance Minerals.
Physical Properties Metric English Comments
Specific Gravity 2.78 g/cc
2.78 g/cc
Bulk Density 0.449 g/cc
0.0162 lb/in³
Loose
1.09 g/cc
0.0394 lb/in³
Tapped
Brightness 90 %
90 %
Hunter Rd, dry
Oil Absorption 24 %
24 %
g oil/100 g filler; ASTM D281
Moisture Absorption at Equilibrium 0.30 %
0.30 %
Loss On Ignition 7.5 %
7.5 %
Particle Size 10 µm
10 µm
Median; Micrometrics Sedigraph 5100
Particle Mesh Size 325 Mesh
325 Mesh
1.0% retained
pH 8.7
8.7
Component Elements Properties Metric English Comments
Al2O3 <= 1.0 %
<= 1.0 %
CaO <= 1.0 %
<= 1.0 %
Fe2O3 <= 1.0 %
<= 1.0 %
MgO 30 %
30 %
SiO2 60 %
60 %