Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.5 µm | 0.5 µm | mean |
PPT LSF120 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Particle Size | 0.5 µm | 0.5 µm | mean |
PPT LSF16 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Particle Size | 0.5 µm | 0.5 µm | mean |
PPT LSF180 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Particle Size | 0.5 µm | 0.5 µm | mean |
PPT LSF220 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Particle Size | 0.5 µm | 0.5 µm | mean |
PPT LSF25 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Particle Size | 0.5 µm | 0.5 µm | mean |
PPT LSF400 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |
|||
Particle Size | 0.5 µm | 0.5 µm | mean |
PPT LSF50 Low Sintering Temperature Ferrite Powder Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4.. |