Material Notes:
Uses: Low Temperature Co-fired Ceramic Components (LTCC), Multi-Layer Chip Inductors (MLCI), Chip Beads (EMI Suppressors)Electromagnetic proerties reported were tested on sintered toroids with a HP4294A.
Physical Properties Metric English Comments
Bulk Density 3.20 g/cc
0.116 lb/in³
pressed
Density 5.20 g/cc
0.188 lb/in³
Sintered
Particle Size 0.5 µm
0.5 µm
mean
Specific Surface Area 5.5 m²/g
5.5 m²/g
Thermal Properties Metric English Comments
Shrinkage 15.5 %
15.5 %
Electrical Properties Metric English Comments
Curie Temperature 500 °C
932 °F
Processing Properties Metric English Comments
Moisture Content 0.30 %
0.30 %
Sintering Temperature 900 °C

@Time 7200 sec
1650 °F

@Time 2.00 hour
Descriptive Properties Value Comments
Initial Permeability, µi 16
Q Factor (w/ 10 turns) 125
Test Frequency 10 MHz