Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 0.750 µm | 0.750 µm | Average Stokes Equivalent Diameter |
KaMin Polyplate® P Kaolin Clay - Delaminated Polyplate® P is a high brightness, delaminated clay intended for use in latex paints, water flexography inks, water-based adhesives or water-based systems where increased hiding, tinting strength.. |
|||
Particle Size | 0.750 µm | 0.750 µm | Average Stokes Equivalent Diameter |
KaMin Polyplate® P01 Kaolin Clay - Delaminated Polyplate® P01 is a milled, high brightness, large particle size delaminated kaolin, intended for use in solvent and water-borne coatings, inks, and adhesives. The high aspect ratio of the large .. |
|||
Particle Size | 0.750 µm | 0.750 µm | Average Stokes Equivalent Diameter |
KaMin Polyfil® DL Kaolin Clay - Delaminated Large, platy delaminated clay that reduces gas/vapor permeability, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, MasterBatchInform.. |