Large, platy delaminated clay that reduces gas/vapor permeability, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl Rubber, MasterBatchInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.641 - 0.753 g/cc
0.0231 - 0.0272 lb/in³
Loose
Solids Content 67 - 69 %
67 - 69 %
Slurry
Brightness 87.5 - 89 %
87.5 - 89 %
Reflectance (TAPPI)
Oil Absorption 45 %
45 %
Fineness >= 4
>= 4
Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Size 0.750 µm
0.750 µm
Average Stokes Equivalent Diameter
3.20 µm
3.20 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6 - 8
6 - 8
100 g/250 ml H2O Slurry
Specific Surface Area 15.0 m²/g
15.0 m²/g
BET
Brookfield Viscosity 450 cP

@Temperature 25.0 °C
450 cP

@Temperature 77.0 °F
20 RPM
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Forms Dry, Slurry
Shipping Point Macon, GA