Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 1.50 µm | 1.50 µm | Median (Malvern Laser) |
KaMin KaMin® 2000C Kaolin Clay - Calcined Highest brightness, smallest particle size, calcined kaolin clay, more cost -effective Ti02 extender than KaMin® 70C.Industry: Paint & CoatingsUses: Architectural Coatings, Industrial Coatings, F.. |
|||
Particle Size | 1.50 µm | 1.50 µm | Median (Malvern Laser) |
KaMin KaMin® 90 Kaolin clay - Waterwashed KaMin® 90 is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90 is ideally suited for solvent and water-borne paint, ink and adhesive applicati.. |
|||
Particle Size | 1.50 µm | 1.50 µm | Median (Malvern Laser) |
KaMin KaMin® 90B Kaolin Clay - Waterwashed KaMin® 90B is a high brightness, fine particle size, general-purpose filler with moderate water demand. KaMin® 90B is ideally suited for water-borne applications where high gloss, holdout and .. |
|||
Particle Size | 1.50 µm | 1.50 µm | Median (Malvern Laser) |
KaMin Polyfil® 90 Kaolin Clay - Calcined Highest brightness, smallest particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, Butyl Rubber, General Plastics, Polyolefins/PVC, Thermoset, Thermo.. |
|||
Particle Size | 1.50 µm | 1.50 µm | Median (Malvern Laser) |
KaMin Polyfil® F Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® F offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® F is a moderate brightness water .. |
|||
Particle Size | 1.50 µm | 1.50 µm | Median (Malvern Laser) |
KaMin Polyfil® FB Kaolin Clay - Waterwashed Water washed kaolin clays such as Polyfil® FB offer acid resistance, reinforcement, neutral pH, and extremely low crystalline silica and salt content. Polyfil® FB is a moderate brightness wate.. |
|||
Particle Size | 1.50 µm | 1.50 µm | Median (Malvern Laser) |
KaMin Polyfil® WC-426 Kaolin Clay - Calcined Fine particle size vinyl-functional calcined clay for outstanding wet electricals and long term stability in wire and cable applications.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rub.. |
|||
Particle Size | 1.50 - 2.50 µm | 1.50 - 2.50 µm | Average value: 1.83 µm Grade Count:3 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Blow Molding Grade". Each property range of values reported is .. |
|||
Particle Size | 1.50 - 2.50 µm | 1.50 - 2.50 µm | Average value: 1.83 µm Grade Count:3 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Sheeting Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Sheeting Grade". Each property range of values reported is mini.. |