Overview of materials for Linear Low Density Polyethylene (LLDPE), Sheeting Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Sheeting Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Linear Low Density Polyethylene (LLDPE), Sheeting Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Sheeting Grade". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.920 - 1.86 g/cc
0.0332 - 0.0672 lb/in³
Average value: 1.26 g/cc Grade Count:7
Particle Size 1.50 - 2.50 µm
1.50 - 2.50 µm
Average value: 1.83 µm Grade Count:3
Environmental Stress Crack Resistance >= 2000 hour

@Temperature 50.0 - 50.0 °C
>= 2000 hour

@Temperature 122 - 122 °F
Average value: 2000 hour Grade Count:2
Melt Flow 0.500 - 8.00 g/10 min
0.500 - 8.00 g/10 min
Average value: 2.39 g/10 min Grade Count:7
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 21.4 - 32.0 MPa
3100 - 4640 psi
Average value: 27.8 MPa Grade Count:3
Processing Properties Metric English Comments
Moisture Content 0.100 %
0.100 %
Average value: 0.100 % Grade Count:3