Physical Properties Metric English Comments
Particle Size 10.0 - 25.0 µm
10.0 - 25.0 µm
D 0.1, SATP-114, Malvern method
Raschig Group PiMC 1221 High gloss
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Particle Size 10.0 - 25.0 µm
10.0 - 25.0 µm
D 0.1, SATP-114, Malvern method
Raschig Group PiMC 1241 Sanitary, uni color
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Particle Size 10.0 - 25.0 µm
10.0 - 25.0 µm
D 0.1, SATP-114, Malvern method
Raschig Group PiMC 1249 Sanitary, mix color
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Particle Size 10.0 - 25.0 µm
10.0 - 25.0 µm
D 0.1, SATP-114, Malvern method
Raschig Group PiMC 1841 Metallic colors
Adding metallic effect pigments to powder coatings gave rise to several application problems such as “spitting”. Synres-Almoco’s Metallic PiMC 1841 ensures easy processing and homogeneous surface..
Particle Size 10.0 - 25.0 µm
10.0 - 25.0 µm
D 0.1, SATP-114, Malvern method
Raschig Group PiMC 1949 Granite colors
PiMC is a Powder in-Mould Coating designed to improve the surface quality, durability and aesthetic appearance of SMC/BMC products. The PiMC is electro statically sprayed onto the heated mould surfa..
Particle Size 10.0 - 70.0 µm
10.0 - 70.0 µm
Average value: 35.0 µm Grade Count:3
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Particle Size 10.0 - 710 µm
10.0 - 710 µm
Average value: 175 µm Grade Count:16
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i..
Particle Size 10.0 - 675 µm
10.0 - 675 µm
Average value: 314 µm Grade Count:30
Overview of materials for Polytetrafluoroethylene (PTFE) Powder
This property data is a summary of similar materials in the MatWeb database for the category "PTFE Powder". Each property range of values reported is minimum and maximum values of appropriate MatWeb..