Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), UHMW PE Ultra High Molecular Weight
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 0.920 - 1.45 g/cc
0.0332 - 0.0524 lb/in³
Average value: 0.946 g/cc Grade Count:147
Water Absorption 0.000 - 0.200 %
0.000 - 0.200 %
Average value: 0.0538 % Grade Count:50
Moisture Absorption at Equilibrium 0.000 - 0.200 %
0.000 - 0.200 %
Average value: 0.0624 % Grade Count:38
Water Absorption at Saturation 0.000 - 0.200 %
0.000 - 0.200 %
Average value: 0.0434 % Grade Count:67
Particle Size 10.0 - 710 µm
10.0 - 710 µm
Average value: 175 µm Grade Count:16
Viscosity Test 470 - 4300 cm³/g
470 - 4300 cm³/g
Average value: 2730 cm³/g Grade Count:8
Environmental Stress Crack Resistance 300 - 600 hour
300 - 600 hour
Average value: 500 hour Grade Count:3
>= 600 hour

@Temperature 50.0 - 50.0 °C
>= 600 hour

@Temperature 122 - 122 °F
Average value: 700 hour Grade Count:4
Oxidative Induction Time (OIT) >= 50.0 min

@Temperature 210 - 210 °C
>= 50.0 min

@Temperature 410 - 410 °F
Average value: 50.0 min Grade Count:1
Molecular Weight 300000 - 9.20e+6 g/mol
300000 - 9.20e+6 g/mol
Average value: 4.97e+6 g/mol Grade Count:39
Melt Flow 0.100 - 12.0 g/10 min
0.100 - 12.0 g/10 min
Average value: 3.08 g/10 min Grade Count:18
Outgassing - Total Mass Loss 0.140 %
0.140 %
Average value: 0.140 % Grade Count:16
Surface Tension 55.0 dynes/cm
55.0 dynes/cm
Average value: 55.0 dynes/cm Grade Count:6
Mechanical Properties Metric English Comments
Hardness, Shore D 54.0 - 120
54.0 - 120
Average value: 63.6 Grade Count:127
Ball Indentation Hardness 24.0 - 57.0 MPa
3480 - 8270 psi
Average value: 36.9 MPa Grade Count:48
Tensile Strength, Ultimate 16.0 - 4200 MPa
2320 - 609000 psi
Average value: 74.0 MPa Grade Count:86
35.0 - 35.0 MPa

@Temperature 32.0 - 32.0 °C
5080 - 5080 psi

@Temperature 89.6 - 89.6 °F
Average value: 35.0 MPa Grade Count:1
Tensile Strength, Yield 0.130 - 40.0 MPa
18.9 - 5800 psi
Average value: 18.4 MPa Grade Count:80
Elongation at Break 25.0 - 800 %
25.0 - 800 %
Average value: 219 % Grade Count:132
Elongation at Yield 8.00 - 350 %
8.00 - 350 %
Average value: 27.3 % Grade Count:29
Creep Strength 3.20 - 13.0 MPa
464 - 1890 psi
Average value: 9.74 MPa Grade Count:29
Modulus of Elasticity 0.300 - 1.30 GPa
43.5 - 189 ksi
Average value: 0.720 GPa Grade Count:75
Flexural Yield Strength 11.0 - 40.0 MPa
1600 - 5800 psi
Average value: 21.1 MPa Grade Count:42
Flexural Modulus 0.400 - 1.45 GPa
58.0 - 210 ksi
Average value: 0.796 GPa Grade Count:35
Compressive Yield Strength 4.00 - 82.7 MPa
580 - 12000 psi
Average value: 14.5 MPa Grade Count:56
Compressive Modulus 0.290 - 0.689 GPa
42.0 - 100 ksi
Average value: 0.557 GPa Grade Count:25
Shear Strength 33.1 MPa
4800 psi
Average value: 33.1 MPa Grade Count:9
Izod Impact, Notched 4.00 - 5340 J/cm
7.50 - 10000 ft-lb/in
Average value: 13.0 J/cm Grade Count:29
Izod Impact, Unnotched 0.641 J/cm - NB
1.20 ft-lb/in - NB
Average value: 0.641 J/cm Grade Count:6
5338.47 - 5338.47 J/cm

@Temperature -40.0 - -40.0 °C
10001.1 - 10001.1 ft-lb/in

@Temperature -40.0 - -40.0 °F
Grade Count:1
Izod Impact, Notched (ISO) 12.0 - 100000 kJ/m²
5.71 - 47600 ft-lb/in²
Average value: 110 kJ/m² Grade Count:14
Charpy Impact Unnotched 1.00 J/cm² - NB
4.76 ft-lb/in² - NB
Average value: 3.77 J/cm² Grade Count:30
Charpy Impact, Notched 2.50 J/cm² - NB
11.9 ft-lb/in² - NB
Average value: 11.7 J/cm² Grade Count:57
3.00 - 3.00 J/cm²

@Temperature -20.0 - -20.0 °C
14.3 - 14.3 ft-lb/in²

@Temperature -4.00 - -4.00 °F
Average value: 3.00 J/cm² Grade Count:1
Coefficient of Friction 0.0200 - 0.350
0.0200 - 0.350
Average value: 0.143 Grade Count:114
0.180 - 0.180

@Temperature 60.0 - 60.0 °C
0.180 - 0.180

@Temperature 140 - 140 °F
Average value: 0.180 Grade Count:1
Coefficient of Friction, Static 0.0800 - 0.200
0.0800 - 0.200
Average value: 0.148 Grade Count:40
Tensile Creep Modulus, 1 hour 370 - 550 MPa
53700 - 79800 psi
Average value: 446 MPa Grade Count:7
Tensile Creep Modulus, 1000 hours 180 - 270 MPa
26100 - 39200 psi
Average value: 229 MPa Grade Count:7
K Factor (Wear Factor) 1.00e-9 - 110
1.00e-9 - 110
Average value: 75.7 Grade Count:7
Limiting Pressure Velocity 0.0500 - 0.210 MPa-m/sec
1430 - 6000 psi-ft/min
Average value: 0.0852 MPa-m/sec Grade Count:38
Compression Set 1.10 - 1.60 %

@Temperature 80.0 - 80.0 °C
1.10 - 1.60 %

@Temperature 176 - 176 °F
Average value: 1.35 % Grade Count:1
Thermal Properties Metric English Comments
CTE, linear 20.0 - 200 µm/m-°C
11.1 - 111 µin/in-°F
Average value: 191 µm/m-°C Grade Count:110
Specific Heat Capacity 1.84 - 2.30 J/g-°C
0.440 - 0.550 BTU/lb-°F
Average value: 1.87 J/g-°C Grade Count:8
Thermal Conductivity 0.330 - 4.00 W/m-K
2.29 - 27.8 BTU-in/hr-ft²-°F
Average value: 0.462 W/m-K Grade Count:60
Melting Point 127 - 255 °C
260 - 491 °F
Average value: 136 °C Grade Count:101
Maximum Service Temperature, Air 70.0 - 135 °C
158 - 275 °F
Average value: 85.4 °C Grade Count:103
Deflection Temperature at 0.46 MPa (66 psi) 65.0 - 95.0 °C
149 - 203 °F
Average value: 71.2 °C Grade Count:14
Deflection Temperature at 1.8 MPa (264 psi) 42.0 - 47.0 °C
108 - 117 °F
Average value: 44.3 °C Grade Count:51
Vicat Softening Point 76.0 - 270 °C
169 - 518 °F
Average value: 92.7 °C Grade Count:16
Electrical Properties Metric English Comments
Electrical Resistivity 100 - 1.00e+18 ohm-cm
100 - 1.00e+18 ohm-cm
Average value: 1.42e+16 ohm-cm Grade Count:81
Surface Resistance 100 - 1.00e+15 ohm
100 - 1.00e+15 ohm
Average value: 1.07e+14 ohm Grade Count:83
Dielectric Constant 2.10 - 3.00
2.10 - 3.00
Average value: 2.54 Grade Count:30
Dielectric Strength 27.6 - 100 kV/mm
701 - 2540 kV/in
Average value: 54.8 kV/mm Grade Count:49
Dissipation Factor 0.000190 - 0.00100
0.000190 - 0.00100
Average value: 0.000578 Grade Count:22
Dielectric Loss Index 0.000100 - 0.00100
0.000100 - 0.00100
Average value: 0.000317 Grade Count:8
Arc Resistance 180 - 240 sec
180 - 240 sec
Average value: 210 sec Grade Count:3
Comparative Tracking Index 600 V
600 V
Average value: 600 V Grade Count:12
Users viewing this material also viewed the following: