Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 90 - 110 µm | 90 - 110 µm | Mean |
SPHERE ONE EXTENDOSPHERESâ„¢ SL-150 Hollow Spheres EXTENDOSPHERESâ„¢ SL are white, low-cost, low-density ceramic hollow spheres.Applications: With a density of 0.73 g/cc and a crush strength of 3,000 psi, these hollow spheres are ideal for use in.. |