Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SPHERE ONE EXTENDOSPHERESâ„¢ SL-150 Hollow Spheres

Category Ceramic , Oxide , Silicon Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Sphere One Inc
Trade Name EXTENDOSPHERES™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SPHERE ONE EXTENDOSPHERESâ„¢ SL-150 Hollow Spheres.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EXTENDOSPHERESâ„¢ SL are white, low-cost, low-density ceramic hollow spheres.Applications: With a density of 0.73 g/cc and a crush strength of 3,000 psi, these hollow spheres are ideal for use in coatings, sealants, caulks and other applications where low shrinkage, lightweight and white particles are desired.Information provided by Sphere One Inc.
Physical Properties Metric English Comments
Bulk Density 0.400 g/cc
0.0145 lb/in³
Density 0.730 g/cc
0.0264 lb/in³
Particle Size 10 - 150 µm
10 - 150 µm
90 - 110 µm
90 - 110 µm
Mean
Mechanical Properties Metric English Comments
Hardness, Mohs 5.0
5.0
Compressive Strength 20.7 MPa
3000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1700 °C
3090 °F
Deformation temp
Component Elements Properties Metric English Comments
Al2O3 38.5 %
38.5 %
Fe2O3 0.50 %
0.50 %
SiO2 59 %
59 %
TiO2 1.7 %
1.7 %
Descriptive Properties Value Comments
Color Off White
Physical Form Free-Flowing Powder
Shell Thickness Approx. 10% of diameter
Users viewing this material also viewed the following: