Particle Size 70 - 120 µm
70 - 120 µm
Mean Granulate Size
Nabaltec GRANALOX® NM 9510 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 80 - 120 µm
80 - 120 µm
Median Grain Diameter
Nabaltec GRANALOX® NM 9620 F Ceramic Bodies
Nabaltec`s GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 70 - 120 µm
70 - 120 µm
Mean Granulate Size
Nabaltec GRANALOX® NM 9634 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 80 - 120 µm
80 - 120 µm
Mean Granulate Size
Nabaltec GRANALOX® NM 9916 F Ceramic Body
Nabaltec's GRANALOX® Ceramic bodies are produced under rigid quality control of green and sintered density, shrinkage, porosity, loss on ignition and granulate size. The properties of the corundum ..
Particle Size 60 - 120 µm
60 - 120 µm
mesh.
Oceanchem Group Xanthan Gum Oil Drilling Grade
Information Provided by Oceanchem Group
Particle Size 5.0 - 120 µm
5.0 - 120 µm
Potters Industries Q-Cel® 7028 Hollow Engineered Glass Microspheres