Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Particle Size = 260 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size 100 - 260 µm
100 - 260 µm
Shandong Dongyue Polymer DF-101 PTFE Molding Powder (Medium Particle Size)
Usage: Can be processed to film, sheet, rob, gasket, axletree and presintered material.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE shou..