Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 125 - 315 µm | 125 - 315 µm | 0.65 |
Arkema Group OREVAC® 18350P Grafted Maleic Anhydride Polyethylene OREVAC 18350P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE and HDPE coating for steel pipeline. It is mainly used in pipe coating to have good adhesion pe.. |
|||
Particle Size | 125 - 315 µm | 125 - 315 µm | 80-90% |
Arkema Group OREVAC® 18510P Grafted Maleic Anhydride Polyethylene OREVAC 18510P is a maleic anhydride grafted polyethylene used in the manufacturing of three layer MDPE or HDPE coating for steel pipeline. It is a powder product. OREVAC 18510P is mainly used in pip.. |