Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 35 - 65 µm | 35 - 65 µm | d50 |
Magyar Aluminum ALOLT 1AF Aluminum Hydroxide Dry type |
|||
Particle Size | 35 - 45 µm | 35 - 45 µm | |
H.C. Starck Amperit® 140.1 Tungsten (W) HS Number: 81011000 |
|||
Particle Size | 35 - 41 µm | 35 - 41 µm | MV |
H.C. Starck Amperit® 554.074 Tungsten Carbide-Cobalt-Chromium 86-10-4 (WC-Co-Cr) |
|||
Particle Size | 35 - 55 µm | 35 - 55 µm | |
Lucite International Colacryl ® TS1742 Acrylic Dental Resin Lucite® Colacryl® TS1742 is a plasticiser free, ethyl methacrylate based resin aimed at the formulation of heat-cured, soft materials, such as ear moulds, where it is well suited to use with C.. |
|||
Particle Size | 35 µm | 35 µm | Mean Value, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 702 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | <= 35 µm | <= 35 µm | average; ISO 1624 |
SolVin 561SF Vinyl Chloride - Vinyl Acetate copolymer Paste - filler Made by suspension polymerization.
APPLICATIONS
This resin has been especially developed for automotive mastics.Information provided by SolVin. |
|||
Particle Size | 35 µm | 35 µm | Average Mean |
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-150 Hollow Spheres EXTENDOSPHERESâ„¢ XOL-150 are white aluminosilicate multicellular hollow spheres. The density of this product is 0.30 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-150 hollo.. |
|||
Particle Size | 35 µm | 35 µm | |
Silberline Aquasil® "BP" 3622 Silberline has specifically created Aquasil® BP grades for aqueous architectural and industrial maintenance coatings. This family offers a cost-effective alternative for achieving stability and .. |
|||
Particle Size | 35 µm | 35 µm | |
Silberline Dedusted Flake Series DF-3622 Aluminum Flake DF-3622 Dedusted Aluminum Flake is manufactured by incorporating a small amount of Teflonâ„¢ with uncoated aluminum pigment, and then, through further processing, is provided in a dry, non-dustin.. |
|||
Particle Size | 35 µm | 35 µm | |
Silberline Sparkle Silver® 3622 Sparkle Silver® 3622 is a coarse, regular purity, non-leafing aluminum pigment. It is characterized by high sparkle, white face color, deep flop and low opacity.Applications: Automotive; General .. |
|||
Particle Size | 35 µm | 35 µm | Before Conversion |
Silberline Sparkle Silvet® 797-20-J Sparkle Silvet® "J" pigments are leafing and non-leafing aluminum pigment pellets designed for ease of handling and incorporation in solvent borne flexographic and gravure ink formulations. The p.. |
|||
Particle Size | 35 µm | 35 µm | |
Silberline Sparkle Silvex® 793-20-C Sparkle Silvex® C grades are aluminum pigment flakes dampened with a plasticizer to help prevent the individual flakes from becoming airborne during handling and processing. They are well suited .. |
|||
Particle Size | 35 µm | 35 µm | Mean Value, Laser diffraction; QSOP-5&75 |
Shamrock Technologies Fluoro T® 602 Thermoplastic Grade PTFE Additive The addition of micronized polytetrafluoroethylene (PTFE) powder to polymeric resins provides greatly increased resistance to surface wear and abrasion. PTFE has a very low coefficient of friction .. |
|||
Particle Size | 35 µm | 35 µm | |
Silberline Tufflake® 2722 Tufflake® aluminum pigments are circulation-resistant, specifically designed to withstand mechanical forces and maintain their target appearance. They are primarily used in automotive coating app.. |
|||
Particle Size | 35 µm | 35 µm | Thin Section Crystal Size |
CoorsTek Dura-Z™ MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 35 µm | 35 µm | Average Crystal Size - Thin Section Test |
CoorsTek TTZ (Dura-Z™) MgO Partially Stabilized Zirconia Thermal Shock Delta Tc = 350°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Particle Size | 35 µm | 35 µm | Laser Method (Dry) |
Daikin POLYFLON M-111 PTFE Molding Powder, Fine Cut Fine cut powder.Processing Methods: Compression molding.Features: Produces moldings with extremely smooth and fine surface. Suited to making packing and gaskets since moldings have an especially go.. |
|||
Particle Size | <= 35 µm | <= 35 µm | Max |
CIMBAR CIMBAR™ PC Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Size | 35 - 45 µm | 35 - 45 µm | Average; ATO 40-41-0 (Coulter Counter) |
Arkema Group ORGASOL® 1002 ES 4 Nat 1 Polyamide 6 Information provided by Arkema Group |
|||
Particle Size | 35 - 55 µm | 35 - 55 µm | D(0.5) |
Akzo Nobel Expancel® 091 WE 40 d24 Wet expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 35 - 55 µm | 35 - 55 µm | D(0.5) |
Akzo Nobel Expancel® 461 DE 40 d25 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 35 - 55 µm | 35 - 55 µm | D(0.5) |
Akzo Nobel Expancel® 461 DET 40 d25 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 35 - 100 µm | 35 - 100 µm | D10-D90 |
ALM PA-640-GSL Filled Nylon 12 Prototyping Polymer This carbon fiber/glass sphere filled composite is an easy to process, extremely light weight filled PA 12 material.Improved dimensional stability, recyclability, and increased stiffness.Good Z dire.. |
|||
Particle Size | 35 µm | 35 µm | 50th% |
3M S22 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Particle Size | 35 - 55 µm | 35 - 55 µm | D(0.5) |
Akzo Nobel Expancel® 091 DE 40 d30 Dry expanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 35 - 45 µm | 35 - 45 µm | D(0.5) |
Akzo Nobel Expancel® 091 DU 140 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Particle Size | 35 - 100 µm | 35 - 100 µm | D10-D90 |
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized.. |
|||
Particle Size | 35 µm | 35 µm | Before Conversion |
Silberline Sparkle Silvet® 790-20-E Sparkle Silvet® E grades are economical aluminum pigments provided in pellet form for easy handling and incorporation. They are composed of 80% aluminum pigment and 20% polyolefin and are compatibl.. |
|||
Particle Size | 35 µm | 35 µm | Before Conversion |
Silberline Sparkle Silvet® 797-30-E1 Sparkle Silvet® E1 grades are easy to disperse and are compatible with a variety of polymers, particularly polyolefins. They are typically used to make concentrates or compounds for use in final pr.. |
|||
Particle Size | 35 µm | 35 µm | |
Lucite International Colacryl ® P2601 Specialty Polystyrene Resin Cross-linked polystyrene resins have much higher thermal stability than conventional thermoplastic acrylic resins. Colacryl® P2601 is stable up to around 300°C.Suggested Uses:This product is usual.. |