Akzo Nobel Expancel® 091 WE 40 d24 Wet expanded microspheres

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer Akzo Nobel, Expancel
Trade Name Expancel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akzo Nobel Expancel® 091 WE 40 d24 Wet expanded microspheres.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the thermoplastic shell softens and the gas increases its pressure, resulting in an expansion of the spheres.Applications: Paints and crack fillers
Physical Properties Metric English Comments
Density 0.0240 - 0.0270 g/cc
0.000867 - 0.000975 lb/in³
Particle Size 35 - 55 µm
35 - 55 µm
D(0.5)
Descriptive Properties Value Comments
Solid Content 15 ± 2
Solvent Resistance 5
Scale of 1 to 5