Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | 6.70 µm | 6.70 µm | Median (Malvern Laser) |
KaMin Polyplate® HMT Kaolin Clay - Delaminated Polyplate® HMT is a high brightness, very high aspect ratio, delaminated kaolin, intended for use in water-borne coatings, adhesives, and sealants. The large, platy structure of Polyplate® HMT.. |
|||
Particle Size | 6.70 µm | 6.70 µm | Median (Malvern Laser) |
KaMin Polyfil® DLX Kaolin Clay - Delaminated Polyfil DLX is a large particle size, very high aspect ratio, delaminated clay that reduces gas and vapor permeability. It is a type of water washed clay which is processed to have a high aspect rat.. |