Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

KaMin Polyplate® HMT Kaolin Clay - Delaminated

Category Ceramic , Clay , Kaolin Clay
Manufacturer KaMin LLC
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KaMin Polyplate® HMT Kaolin Clay - Delaminated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polyplate® HMT is a high brightness, very high aspect ratio, delaminated kaolin, intended for use in water-borne coatings, adhesives, and sealants. The large, platy structure of Polyplate® HMT imparts increased hide, tinting strength, enamel holdout, crack resistance, and reinforcement properties in water based systems.Industry: Paint & Coatings, Adhesives & Sealants, Rubber & PlasticUses: Architectural Coatings, Industrial Coatings, Wood Coatings, Flat/Matte, Satin, Primer, Water Based, Non-Black RubberInformation provided by KaMin LLC.
Physical Properties Metric English Comments
Specific Gravity 2.60 g/cc
2.60 g/cc
Bulk Density 0.641 - 0.721 g/cc
0.0231 - 0.0260 lb/in³
Loose
Solids Content 66 - 68 %
66 - 68 %
Slurry
Brightness 87.5 - 89 %
87.5 - 89 %
Reflectance (TAPPI)
Oil Absorption 42 %
42 %
Fineness >= 4
>= 4
Hegman Grind
Moisture Absorption at Equilibrium <= 1.5 %
<= 1.5 %
As Produced
Particle Size 1.20 µm
1.20 µm
Average Stokes Equivalent Diameter
6.70 µm
6.70 µm
Median (Malvern Laser)
Particle Mesh Size 325 Mesh
325 Mesh
0.005% Retained
pH 6 - 8
6 - 8
100 g/250 ml H2O Slurry
Specific Surface Area 12.0 m²/g
12.0 m²/g
BET
Brookfield Viscosity 800 cP

@Temperature 25.0 °C
800 cP

@Temperature 77.0 °F
20 RPM
Descriptive Properties Value Comments
Bulking Value 21.7 lb.gal
CAS Number 1332-58-7
Crystalline Silica (quartz) <0.1%
Physical Forms Dry, Slurry
Shipping Point Macon, GA