Polymer Property : Particle Size = 8000 µm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast CURON 110 C AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast CURON 110 C Dense Refractory Castable
Description: Curon 110 C is a coarse castable. Application: covers for anode baking furnaces.Remarks: These values apply to cast products.Information provided by Gouda Vuurvast.
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast CURON 120 C Dense Refractory Castable
Description: A general purpose castable for use up to 1200°C under normal operating conditions. Curon 120 C has good thermal shock resistance.Remarks: These values apply to cast products.Informat..
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast CURON 120 LC AL Dense Refractory Castable
Description: Because of special addition this coarse castable shows a very good resistance against liquid aluminum metal.Remarks: These values apply to cast products.Information provided by Gouda Vu..
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast CURON 160 HC Dense Refractory Castable
Description: Because of the selection of raw materials, this castable has a high volume stability and keeps its strength up to high temperatures. In addition, Curon 160 HC has an excellent thermal s..
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast GOLITE 135 RL C Refractory Insulating Castable
Description: Golite 135 RL C is a coarse low iron light weight castable and combines a good mechanical strength with a low density and a low thermal conductivity.Remarks: These values apply to cast ..
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast VIBRON 140 C RAPID Dense Vibrating Refractory Castable
Description: Vibron 140 C Rapid is a low cement castable, based on high quality coarse chamotte grog. Because of special additives this castable is special suited for a faster heating schedule.Remar..
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast CURON 130 HRC AL Dense Refractory Castable
Description: Because of special addition this castable is used for the walls above the liquid level in aluminum melting furnaces.Remarks: These values apply to cast products.Information provided by ..
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast CURON 130 HRC Dense Refractory Castable
Description: A coarse, low iron castable for use up to 1300°C under normal operation conditions, also usable under reducing circumstances. Curon 130 HRC has a good thermal shock resistance becaus..
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast CURON 160 HSC Dense Refractory Castable
Description: Curon 160 HSC is a coarse abrasion resistant castable to be used up to 1600°C in reducing conditions.Remarks: These values apply to cast products.Information provided by Gouda Vuurva..
Particle Size <= 8000 µm
<= 8000 µm
Grain Size
Gouda Vuurvast CURON 100 C Dense Refractory Castable
Description: Curon 100 C can be applied up to 1000°C, under normal operating conditions and is especially applied in the bottom of electrolytic cells in the aluminum industry.Remarks: These values ..