Polymer Property : Specific Surface Area = 0.833 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 0.833 m²/g
0.833 m²/g
Blaine
SGL Carbon Group CF 3100 Graphite Filler
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..