Physical Properties Metric English Comments
Specific Surface Area 1.4 m²/g
1.4 m²/g
BET
Nyco NYGLOS® 8 Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
Specific Surface Area 1.4 m²/g
1.4 m²/g
BET
Nyco RRIMGLOS® II Wollastonite
This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make..
Specific Surface Area <= 1.4 m²/g
<= 1.4 m²/g
BET
Magyar Aluminum ALO-DN-3S Alumina
Ground Alumina
Specific Surface Area 1.4 m²/g
1.4 m²/g
BET
Nyco ULTRAFIBRE® II Wollastonite
Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br..