Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 1.4 m²/g | 1.4 m²/g | BET |
Nyco NYGLOS® 8 Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Specific Surface Area | 1.4 m²/g | 1.4 m²/g | BET |
Nyco RRIMGLOS® II Wollastonite This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology make.. |
|||
Specific Surface Area | <= 1.4 m²/g | <= 1.4 m²/g | BET |
Magyar Aluminum ALO-DN-3S Alumina Ground Alumina |
|||
Specific Surface Area | 1.4 m²/g | 1.4 m²/g | BET |
Nyco ULTRAFIBRE® II Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |