Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 16.0 m²/g | 16.0 m²/g | BET |
KaMin KaMin® 2000C Kaolin Clay - Calcined Highest brightness, smallest particle size, calcined kaolin clay, more cost -effective Ti02 extender than KaMin® 70C.Industry: Paint & CoatingsUses: Architectural Coatings, Industrial Coatings, F.. |
|||
Specific Surface Area | 16.0 m²/g | 16.0 m²/g | BET |
KaMin KaMin® 80 Kaolin Clay - Waterwashed KaMin® 80 is an economical, general purpose water-washed kaolin, with intermediate brightness. It is suitable for use in water-borne, solvent-borne and solvent-free paint, ink, and adhesive appli.. |
|||
Specific Surface Area | 16.0 m²/g | 16.0 m²/g | BET |
KaMin Polyfil® X Kaolin Clay - Waterwashed Cost effective, kaolin extender offering improved consistency vs air floated clays, pulverized powder form.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, SMC/BMC, EPDM, Mold.. |
|||
Specific Surface Area | 16.0 m²/g | 16.0 m²/g | BET |
KaMin Polyfil® 90 Kaolin Clay - Calcined Highest brightness, smallest particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber Goods, Butyl Rubber, General Plastics, Polyolefins/PVC, Thermoset, Thermo.. |