Polymer Property : Specific Surface Area = 18.0 m²/g Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Surface Area 18.0 m²/g
18.0 m²/g
BET
KaMin KaMin® 611 Kaolin Clay - Waterwashed
Naturally delaminated clay for use in water-based paints and coatings.Industry: Paint & CoatingsUses: Industrial Coatings, E-Coat, PrimerInformation provided by KaMin LLC.