Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Surface Area | 3.0 - 5.0 m²/g | 3.0 - 5.0 m²/g | BET |
Magyar Aluminum ALOLT 60DLS Aluminum Hydroxide Fine Precipitated Type |
|||
Specific Surface Area | 3.0 - 5.0 m²/g | 3.0 - 5.0 m²/g | BET |
Magyar Aluminum ALOLT 60F Aluminum Hydroxide Fine Precipitated Type |
|||
Specific Surface Area | 3.0 - 5.0 m²/g | 3.0 - 5.0 m²/g | BET |
Magyar Aluminum ALOLT 60P Aluminum Hydroxide Fine Precipitated Type |
|||
Specific Surface Area | 0.50 - 5.0 m²/g | 0.50 - 5.0 m²/g | |
Momentive Performance Materials PolarTherm® PT120 Boron Nitride (BN) Powder Fine Hexagonal BN PowderWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |
|||
Specific Surface Area | 1.0 - 5.0 m²/g | 1.0 - 5.0 m²/g | |
American Elements Iridium Nanoparticles General DescriptionIridium (Ir) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Iridium Particles are typically 20 - 100 nanometers (nm) with s.. |
|||
Specific Surface Area | 1.0 - 5.0 m²/g | 1.0 - 5.0 m²/g | |
American Elements Molybdenum Nanoparticles General DescriptionMolybdenum (Mo) Nanoparticles, nanodots or nanopowder are black high surface area particles. Nanoscale Molybdenum Particles are typically 50 - 100 nanometers (nm) with specific su.. |
|||
Specific Surface Area | 1.0 - 5.0 m²/g | 1.0 - 5.0 m²/g | |
American Elements Titanium Nanoparticles General DescriptionTitanium (Ti) Nanoparticles, nanodots or nanopowder are spherical or faceted high surface area metal particles. Nanoscale Titanium Particles are typically 10 - 80 nanometers (nm) .. |
|||
Specific Surface Area | 1.0 - 5.0 m²/g | 1.0 - 5.0 m²/g | |
American Elements Tungsten Nanoparticles General DescriptionTungsten (W) Nanoparticles, nanodots or nanopowder are black spherical high surface area metal particles. Nanoscale Tungsten Particles are typically 40-80 nanometers (nm) with spe.. |
|||
Specific Surface Area | 3.0 - 5.0 m²/g | 3.0 - 5.0 m²/g | B.E.T. |
ATI Wah Chang Hafnium Oxide S Grade, HfO2 A white, free flowing powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis |
|||
Specific Surface Area | 0.50 - 5.0 m²/g | 0.50 - 5.0 m²/g | |
Momentive Performance Materials PolarTherm® PT670 Boron Nitride (BN) Powder High Density BN AgglomerateWhen used in a variety of polymeric materials, PolarTherm™'s heat dissipating capability helps extend the service life and enhance the reliability of electronic comp.. |