Physical Properties Metric English Comments
Specific Surface Area 9.5 m²/g
9.5 m²/g
Omya OMYACARB® UTF-FL Calcium Carbonate
A high purity, ultrafine, wet ground, surface treated natural calcium carbonate available in dry form.Applications: Plastic applications such as rigid PVC and flexible PVC. Paint applications such a..
Specific Surface Area 9.5 m²/g
9.5 m²/g
BET
TIMCAL TIMREX® MB15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..
Specific Surface Area 9.5 m²/g
9.5 m²/g
BET
TIMCAL TIMREX® MX15 Primary Synthetic Graphite
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all pro..