TIMCAL TIMREX® MB15 Primary Synthetic Graphite

Category Carbon , Graphite , Other Engineering Material , Additive/Filler for Polymer
Manufacturer TIMCAL
Trade Name TIMREX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMCAL TIMREX® MB15 Primary Synthetic Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TIMREX Primary Synthetic Graphite is produced in a unique highly controlled graphitization process which assures narrow specifications and unequalled consistent quality due to: monitoring of all production and processing stages, strict final inspection, and clearly defined development processes.TIMREX Primary Synthetic Graphite shows unique properties thanks to the combination of a consistent purity, perfect crystalline structure and well defined texture.Information provided by TIMCAL
Physical Properties Metric English Comments
Bulk Density 0.0900 g/cc
0.00325 lb/in³
Scott
Particle Size 18 µm
18 µm
d90
Specific Surface Area 9.5 m²/g
9.5 m²/g
BET
Ash 0.060 %
0.060 %
Electrical Properties Metric English Comments
Electrical Resistivity 105 ohm-cm
105 ohm-cm
8% graphite
200 ohm-cm
200 ohm-cm
6% graphite
400 ohm-cm
400 ohm-cm
4.9% graphite
600 ohm-cm
600 ohm-cm
4.2% graphite
Descriptive Properties Value Comments
Aspect Fine black powder
Battery type High-drain AA, AAA
Flexural Strength 6.5 N
4.1% graphite
7 N
5.1% graphite
7.5 N
6.4% graphite
8 N
8% graphite
Graphite 6-7%
Recommended concentration
Particle Shape Anisometric, flakes