Physical Properties Metric English Comments
Molecular Weight 150.69 g/mol
150.69 g/mol
American Elements Tin Oxide Nanopowder
General DescriptionTin Oxide ( SnO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide Parti..