Polymer Property : Molecular Weight = 162.03 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 162.03 g/mol
162.03 g/mol
Solvay Chemicals Sifren® 46 Hexafluoro-1,3-butadiene
Sifren® 46 (C4F6 or Hexafluorobutadiene) C4F6 has a GWP=0 and it is the most advanced etching gas for critical applications. Its low C/F ratio and its insaturations allow achieving the highest as..