Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 162.03 g/mol | 162.03 g/mol | |
Solvay Chemicals Sifren® 46 Hexafluoro-1,3-butadiene Sifren® 46 (C4F6 or Hexafluorobutadiene) C4F6 has a GWP=0 and it is the most advanced etching gas for critical applications. Its low C/F ratio and its insaturations allow achieving the highest as.. |