Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 231.85 g/mol | 231.85 g/mol | |
Reade Advanced Materials Tungsten Oxide Powder (WO2 and WO3) Description: Tungsten oxide is obtained from the minerals sche, wolframite, ferberite. It is insoluble in H2O and acids, but soluble in hot alkalis. Used in the manufacture of tungsten and tungstat.. |
|||
Molecular Weight | 231.85 g/mol | 231.85 g/mol | |
American Elements Tungsten Oxide Nanopowder General DescriptionTungsten Oxide ( WO) Nanopowder or Nanoparticles, nanodots or nanocrystals are spherical or faceted high surface area oxide magnetic nanostructure particles. Nanoscale Tin Oxide P.. |