Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 300000 g/mol | 300000 g/mol | |
Polikim ULPOLEN® 300 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Molecular Weight | 300000 - 9.20e+6 g/mol | 300000 - 9.20e+6 g/mol | Average value: 4.97e+6 g/mol Grade Count:39 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Molecular Weight | 300000 - 900000 g/mol | 300000 - 900000 g/mol | |
Lucite International Colacryl ® B611 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I.. |
|||
Molecular Weight | 300000 - 900000 g/mol | 300000 - 900000 g/mol | |
Lucite International Colacryl ® B866 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based homopolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.. |
|||
Molecular Weight | 300000 - 900000 g/mol | 300000 - 900000 g/mol | |
Lucite International Colacryl ® D1-120 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I.. |
|||
Molecular Weight | 300000 - 500000 g/mol | 300000 - 500000 g/mol | |
Lucite International Colacryl ® TS1326 Acrylic Dental Resin Colacryl® TS1326 is a plasticiser free, ethyl methacrylate based resin aimed at the formulation of temporary crown and bridge materials. It may be used in conjunction with most traditional cold c.. |
|||
Molecular Weight | 300000 - 500000 g/mol | 300000 - 500000 g/mol | |
Lucite International Colacryl ® TS1742 Acrylic Dental Resin Lucite® Colacryl® TS1742 is a plasticiser free, ethyl methacrylate based resin aimed at the formulation of heat-cured, soft materials, such as ear moulds, where it is well suited to use with C.. |
|||
Molecular Weight | 300000 - 900000 g/mol | 300000 - 900000 g/mol | |
Lucite International Colacryl ® TS2027 Acrylic Dental Resin Cold-curing denture repair resin with Methyl Methacrylate based copolymers. Features fast polymerisation, easy mixing, good clarity, short hydroflask cure cycles, and excellent pigment acceptance.I.. |