Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 546 g/mol | 546 g/mol | |
Dow Corning 705 DIFFUSION PUMP FLUID A colorless, penta phenyltrisiloxane, single-component fluid designed for ultrahigh vacuums of 10-10 torr (untrapped) and 10-11 (trapped).Information provided by Dow Corning |