Dow Corning 705 DIFFUSION PUMP FLUID

Category Polymer , Thermoplastic , Siloxane
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 705 DIFFUSION PUMP FLUID.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A colorless, penta phenyltrisiloxane, single-component fluid designed for ultrahigh vacuums of 10-10 torr (untrapped) and 10-11 (trapped).Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc

@Temperature 25.0 °C
1.09 g/cc

@Temperature 77.0 °F
Viscosity Measure 175 cSt
175 cSt
kinetic/kinematic
Molecular Weight 546 g/mol
546 g/mol
Surface Tension 36.5 dynes/cm
36.5 dynes/cm
Thermal Properties Metric English Comments
Heat of Vaporization 118000 J/g

@Temperature 250 °C
50800 BTU/lb

@Temperature 482 °F
Boiling Point 245 °C
473 °F
Flash Point 243 °C
469 °F
open cup
Processing Properties Metric English Comments
Shelf Life 60.0 Month
60.0 Month
Descriptive Properties Value Comments
Ultimate Vacuum (Torr) 1E-11
trapped
1e-9 to 1e-10
untrapped